  "bed_temperature_c": 80.0,
  "brand_name": "Fiberlogy",
  "doi": "10.3390/ma17091988",
  "dtensile_mpa_per_pct_moisture": -15.49,
  "filament_moisture_max_pct": 0.75,
  "filament_moisture_min_pct": 0.17,
  "infill_density_pct": 100.0,
  "infill_pattern": "grid 45 degrees",
  "is_standard_coupon": true,
  "is_training_ready": true,
  "layer_height_mm": 0.19,
  "material_abbreviation": "ABS",
  "material_class": "FFF",
  "material_family": "ABS",
  "material_name": "pure transparent ABS",
  "material_type": "ABS",
  "measurement_confidence": "calculated",
  "moisture_conditioning_path": "absorption",
  "moisture_response_r": -0.993,
  "n_specimens": 5,
  "nozzle_diameter_mm": 0.4,
  "print_orientation": "flat",
  "print_speed_mm_s": 30.0,
  "print_temperature_c": 275.0,
  "printer_model_reported": "Zortrax M200 Plus (closed chamber)",
  "record_created_at": "2026-08-11",
  "record_id": "0d833e1a-5601-59da-98d9-84bc4f64efcb",
  "record_kind": "moisture_response",
  "record_revision": 1,
  "schema_version": "0.1.0",
  "source": "pmc_11084188",
  "source_citation": "pmc_11084188. DOI 10.3390/ma17091988 (CC-BY-4.0)",
  "source_license": "CC-BY-4.0",
  "specimen_standard": "ISO 527",
  "strength_loss_per_pct_moisture": 0.47384521260324264,
  "tensile_strength_mpa": 32.69
}